Randy McCall on mon 10 jul 06


Thanks for all the suggestions. I had 4 pitchers that I put in the oven and
went up to 400 degrees. Looks like it worked. Touched up the pieces. Will
see how it works in the next glaze firing.

Hard to keep your hand steady when using that stuff.......thanks again for
the suggestions.


Randy
South Carolina
Pottery Web site