Hi all,

I am in need (looking for quotes) on the following materials for a special anagama kiln building project in Southern Minnesota with an organization that works with at risk teens:

1000 2600degree Hard Brick Straights 9 x 4.5 x 2.5 inches
75 #1 Arch Brick
200# of castable and mortar
Twenty 12 x 24 inch by 3/4 inch kiln shelves
or twelve 18 x 24 inch 3/4 inch kiln shelves
48 half bricks

I have contacted Donna at Smith Sharp and she has given me a quote. I am looking to see if anyone has any of the materials for sale or knows other sources I may contact for the best price.

Thank you

Tony


Tony Ferguson
...where the sky meets the lake...
Duluth, Minnesota
Artist, Educator, Web Meister
fergyart@yahoo.com
fergy@cpinternet.com
(218) 727-6339
http://www.aquariusartgallery.com
http://www.tonyferguson.net

---------------------------------
How low will we go? Check out Yahoo! Messenger’s low PC-to-Phone call rates.