search  current discussion  categories  glazes - misc 

orange glaze....

updated tue 8 aug 06

 

Karen Sullivan on sun 6 aug 06


Beth...
If what you want is a vibrant orange glaze...
Perhaps look at the Cerdec/Degussa inclusion stains...
An encapsulated color that survives cone 10...
Vibrant yellow, orange, not so interesting red....
They are expensive....but will give consistent
Bright color...better in oxidation than
Reduction...

Good luck.