Karen Sullivan on mon 21 aug 06


Paul....

What you propose sounds incredibly
Complicated....
How about making small hershey kisses
Out of clay....use those as posts...
The weight of the fired object
Will determine how fine a point the
Kiss shape has....
I actually use broken cordorite/mullite
Kiln shelf pieces to prop up work
That is glazed all over...I form a
Tripod support and balance the work...
If the contact area is small between
The object and the post/stilt
It will knock off easily and any
Small mark you can grind off....

Hope that helps...
Karen