Scott Hunnicutt on tue 29 aug 06
Hey all,
Haven't posted in a while and I have a question about a glaze in Robert
Tichane book: Those Celadon Blues.
I like the look of his Kuan glaze but I get confused about when he lists the
formula. He mentions to underfire the glaze and that if the glaze is fired
to maturity that it will not crackle. But no where does he say either the
original cone or what to cone to underfire too. Has anyone made this glaze
if so what cone do you fire to make it crackle? and does anyone have a glaze
recipe for his kuan glaze?
thanks for any replies in advance,
Scott Hunnicutt
beginning potter
| |
|