search  current discussion  categories  glazes - misc 

was runny glaze now fatty tumors

updated wed 13 sep 06

 

claybair on tue 12 sep 06


Kathryn,
See:
http://www.potters.org/subject84766.htm
&
http://www.google.com/search?hl=en&lr=&q=lipomas
&
http://www.google.com/search?hl=en&q=Manganese+Toxicity
I don't think the manganese caused your problem.

Gayle Bair
Bainbridge Island, WA
Tucson, AZ
http://claybair.com

-----Original Message-----
From: Kathryn Hughes

Ron Roy,thanks so much for your answers. They were very helpful. Now onto
something else. Have you encountered any potters who have had are is having
alot of fatty tumors growing along their arms? I think for me it has
something to do when I'd swish the mang carb. with my bare hands up to my
arms before someone told me that it was very poisonous. Idiot me. but I'm
curious to know of any other potters who may have these problems or others.
With warm regards, Kathryn

--