Randy McCall on sun 24 sep 06
I just purchased this book and it has a clear glaze that appears incorrect.
It adds up to 123.3 instead of the stated 100%.
I was wondering if anyone else has this book and know is correct formula for
the clear glaze.
Randy
South Carolina
Pottery Web site
http://members.tripod.com/~McCallJ/index.html
Edouard Bastarache Inc. on sun 24 sep 06
Hello Randy,
divide the whole proportion by 1.233
Later,
Edouard Bastarache
Le Français Volant
The Flying Frenchman
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
www.sorel-tracy.qc.ca/~edouardb/Welcome.html
http://perso.wanadoo.fr/smart2000/index.htm
http://www.pshcanada.com/Toxicology.htm
http://www.flickr.com/photos/30058682@N00/
http://thepottersshop.blogspot.com/
----- Original Message -----
From: "Randy McCall"
To:
Sent: Sunday, September 24, 2006 9:04 AM
Subject: Book - Wheel Thrown Pottery DIY
>I just purchased this book and it has a clear
>glaze that appears incorrect.
> It adds up to 123.3 instead of the stated 100%.
>
> I was wondering if anyone else has this book and
> know is correct formula for
> the clear glaze.
>
>
> Randy
> South Carolina
> Pottery Web site
>
> http://members.tripod.com/~McCallJ/index.html
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or
> change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be
> reached at melpots@pclink.com.
>
| |
|