Randy McCall on fri 20 oct 06
Go to the hardware store and buy some electrical wires that have a
thermostat that are used to put on pipes under the house to keep them from
freezing. They come on only when it gets below freezing. You should be
able to wrap the pugmill in those and keep it in shape.
Randy
South Carolina
Pottery Web site