Hi Mel and folks on Clayart,

Thanks, Mel, for sharing a picture of your iron red glaze. Very very nice.
Now, we will all want to try the Rhodes, etc. combination!!!

I did try a glaze called Rob's, don't know where it came from, we have it in
the Lee Arts Center studio, on Bailey's Red reduction, and got some very nice
results. Also used Steven Hill's Yellow Crystal Glaze on the same red, and got
very nice results with that too.

Thanks too, Mel, for giving us info on Clayart on your web page. I used it
just the other day to find out what was happening, and got the message.

Veena


In a message dated 10/28/2006 6:51:27 PM Eastern Standard Time,
melpots2@VISI.COM writes:
>
> i added a picture of a classic iron red glaze
> that i use. nothing special...bone ash basic.
>
> it is on the clayart page.
> make sure you bookmark that page as
> bill has suggested...if there are any breakdowns
> with clayart..messages will be placed there.
> click below/clayart page.
> mel
>
> from: mel/minnetonka.mn.usa
> website: http://www.visi.com/~melpots/