search  current discussion  categories  materials - frits 

that hunter green recipe: check frit

updated sun 29 oct 06

 

Eleanora Eden on sat 28 oct 06


Hi Nancy,

Please look again at your recipe and see if there is more information
on that frit.

Eleanora

>Hi
>
>I was going through my CDs and browsing old copies of clay art back
>from 98/99 and found a hunter green glaze that I am not sure if
>anyone has shared with you. It is cone 6 ox and is as follows:
>
>Frit 22%
>Strontium Carbonate 16%
>Feldspar 34%
>Wollastonite 12%
>Flint 6%
>OM-4 10%
>
>Bentonite 2%
>Victoria Green mason stain 8%
>
>it cam from Corcoran School of Art by Grace Lewis
>
>Hope it helps
>
>
>
>
>Nancy
>Hilltop Pottery
>
--
Bellows Falls Vermont
www.eleanoraeden.com