i love a variety of batts.

if you only have plastic...well, as was just
mentioned..don't use the heat gun.

i have some great 5/8" particle board batts.
i use them for tall pieces and big things.
they don't warp, bend or break.

masonite and hardiboard bats are great for letting
the pot bleed off some water.

plastic are great for sets...all the same...one after the other.
and i do all of my tap center trimming on a plastibatt.

i just never use plaster...have never used them, so i
just don't..nothing wrong with them, just used other
kinds.
of course i need a few 25 inch bats for those sometimes
thrown big platters.