search  current discussion  categories  techniques - slips 

slipfalls off the pot

updated tue 7 nov 06

 

Pat Southwood on mon 6 nov 06


Hi Carol,
I use white st thomas all the time, a basic slip of 50/50 ball clay and =
china clay + your oxide additions has always worked fine for me
I have to confess to not even weighing it, if i just want white slip, =
just 2 scoops, one of each.
You receipe sounds more like an engobe than a slip.
Best wishes,
Pat Southwood