=?ISO-8859-1?Q?ow=20-=20not=20using=20stains?=

Donna,

Look up Butterscotch in the archieves. It is a cone 6 oxidation satin
matte. I believe the yellow is derived at least partly from titanium. You can
learn more about titanium in The Potter's Dictionary.