Shakeel Abedi on tue 28 nov 06


Hi Folks

I has been raing here for days and will do do so most of December and
January. Pots just don't want to dry.

Is is possible for me to stack them in a kiln and simulate a dry day,
say put the kiln at 140F or so fro a day and let them dry out before
starting the bisque cycle?

--
Shakeel Abedi

Snail Scott on wed 29 nov 06


At 11:00 AM 11/28/2006 +0800, you wrote:
>...Pots just don't want to dry.
>Is is possible for me to stack them in a kiln and simulate a dry day,
>say put the kiln at 140F or so...


Yes, it is. -Snail