Eleanora Eden on wed 6 dec 06
Yikes, yes, you are correct. I meant ^3.
E
>Hi Eleanora,
>
>When you wrote "As soon as cone 1 started to move I adjusted my computer
>to" I think you ment cone 3 started to move right?
>
>Otherwise you would have had to wait for hours for cone 3 to fall.
>
>RR
>
>>Ron and John, and all,
>>
>>Want to report that this made a whole big difference in my most recent
>>firing. I had gone
>>successfully to cone 1 exactly and now wanted to go exactly to cone 3,
>>comparing clay
>>and glaze at both temperatures.
>>
>>It went without a hitch. As soon as cone 1 started to move I adjusted my
>>computer to
>>soak at that point for 15 m then start cool down. On both peep and
>>witness shelf cones, ^ 3 was
>>arching down like in that little video clip, and ^ 4 soldierly upright.
>>
>>Clay and glaze were both fabulous at ^3 so now I am officially going there.
>>
>>Thanks as always,
>>
>>Eleanora
>
>Ron Roy
>RR#4
>15084 Little Lake Road
>Brighton, Ontario
>Canada
>K0K 1H0
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
--
Bellows Falls Vermont
www.eleanoraeden.com
| |
|