stephani stephenson on sat 16 dec 06


to quote tiny elvis
the effect clay body can have on the
glossiness,mattnes even coloration of a glaze is
h-u-u-u-g-e.

man, it's h-u-u-ug-e.

no joke.
fluxes , oxides and solubles in the clay body , as
well as alumina silica content, etc... can make quite
a difference , and ,with regard to commercial bodies,
even among claybodies which are rated for the same
firing temperature and look similar in the bag

Stephani Stephenson
revivalsteph[use@]yahoo.com