search  current discussion  categories  techniques - spraying 

spray painting-house - never!!

updated fri 26 jan 07

 

Sam or Mary Yancy on thu 25 jan 07


Spay painting will leave a "blothchy" job and (guarantee) transfer the spray to almost everthing in the neighborhood that is not covered, especially on a windy day. I once got a car repainted FREE because of "overspray" Plus some healthy dollars.The house painted was over 1/8 mile away. . Even if you could paint the house with spray equipment, It will NEVER have the protective coating of a roller or a paint brush, both which Press the paint into the surface. I am or was a profisional painter using spray equipment, but I NEVER used it to paint a house or other external area. Not worth the effort, the LIABILITY and the quality of the paint job. Sam in daly city NOTE - my oppinion only but take a look at some buildings/houses that were painted with spray equipment...............