***total wet firing/ beyond raku***

updated tue 20 feb 07

 

Frank Colson on mon 19 feb 07


For fun and experimental experiences, here is my published article on TOTAL
WET FIRING. This "eBook" is free! Just scroll to the bottom of :
www.R2D2u.com opening page and download. The B&W photos are lacking clarity,
but you will find how we went through nearly 100 pieces in a "Teacher's
Workshop" to alter the thermal charcter of clay and thansfer
a hand built or wheel thrown pots directly to a pre-heated kiln for "glaze"
firing!


Frank Colson
www.R2D2u.com






----- Original Message -----
From: "arkey03755"
To:
Sent: Sunday, February 18, 2007 9:42 AM
Subject: Re: Glass in Pottery?


very often i have melted glass in the bottom of dishes and in the
indentation of knobs. i used to use crushed discarded botles but
found i had a lot of cracks due to difences in the glass coeff of
expansion. now i buy "frits" from Bullseye glass. all this means is
finely ground glass and all the bu7llseye glass haqs the same coe so
they can all be mixed. i hae gotten some verry interresting effects
using diffents colors. but one must be careful not to use too much as
tthe expansion will cause the pot to crack. so start with a little
and then increase to get the best result.
eleanor arkowitz

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.