ester svensson on thu 22 feb 07
Hello and thanks for the ideas!
we've actually found a machine here in the bazaar which is an agricultural
grinder for wheat and corn and things, that has been adapted, ie the inside
part has been changed to stronger metal, so it can even grind quartz! so
that will let us grind all sorts of stuff. the other option was getting a
ballmill imported from pakistan, but this seems like a cheaper and better
option.
i'll let you know how we get on with it...
thanks again everyone for all the input!
all the best from a sunny Kabul, ( i think spring is finally here!)
ester
On 20/02/07, Megan Mason wrote:
>
> In a message dated 2/19/2007 8:20:17 P.M. Eastern Standard Time,
> mlkrakowski@CITLINK.NET writes:
>
> corn grinders used to grind up clay....having said
> which, I (who knows NOTHING about the technical aspects of this, and make
> no
> claim to knowledge, only curiosity) wonder if out of old truck gears or
> something a grinder could not be made to pulverize the raw clay, crush as
> much of the lime bits as possible, before the whole slaking process
> begins.
>
>
>
> old farm hammer mills work as well
>
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
| |
|