serious glaze breaks

updated wed 14 mar 07

 

Megamelon on mon 12 mar 07


Anybody else look at the Joe Finch Kiln book dumbfounded at some of his =
glaze work? The pieces there are on a red body, and the glaze seems to =
break from blue through green into yellow with the red body showing =
through in places. Could be multiple glazes overlayed, but much of it =
looks seemless.

It's killah.

Anyway- I like the idea that the clay body seems to play a big role =
there. I want to experiment with tenmoku and shino for maximum break =
effects. Any suggestions on ^10 woodfired, colorful, food safe glazes =
that break like that as well?