Stef wrote.....I am using a cone 6 Raku clay and also a cone 6
porcelain paper
clay for Raku. Both work fine for that now I am wondering if they would
work as well with smoke firing..
Hi,
I'm using Soldate 60 bisque fired to C/04, smoking it in a weber BBQ
with saw dust, pine needles and redwood tree droppings, ( are they
needles? ), anything that burns good.Works just fine. Mike Gordon
| |
|