looking for ^6 red & purple -

updated thu 31 oct 96

 

BobWicks@aol.com on sat 19 oct 96

Terri:

You left out a very important figure in the recipe you just sent Sue Hintz.
EPK is absolutely necessary. How much are you using??

Bob

The Storer Family on sun 20 oct 96

BobWicks@aol.com wrote:
>
> ----------------------------Original message----------------------------
> Terri:
>
> You left out a very important figure in the recipe you just sent Sue Hintz.
> EPK is absolutely necessary. How much are you using??
>
> Bob


Sorry about that Bob. EPK should be 4.5 %.

Terri