Valice Raffi on thu 14 aug 97

Hi all,

I'm hoping someone might have a recipe for a dry (or matt) white lichen
glaze, preferably low fire. Does such an animal exist?

An alternative would be similar (dry white) slip or glaze that will "pop
off" in places.

Hoping someone can help.

Gratefully,

Valice in Sacramento

Patrick & Lynn Hilferty on fri 15 aug 97

Valice,

Try this:

Frit 3269 25%
Barium 10%
Nephylene Syenate 25%
Magnesium Carb 25%
EPK 10%
zinc 5%

I got this from Jim Haggerty when I was at Long Beach State.

Patrick


At 10:43 -0400 8/14/97, Valice Raffi wrote:
>----------------------------Original message----------------------------
>Hi all,
>
>I'm hoping someone might have a recipe for a dry (or matt) white lichen
>glaze, preferably low fire. Does such an animal exist?
>
>An alternative would be similar (dry white) slip or glaze that will "pop
>off" in places.
>
>Hoping someone can help.
>
>Gratefully,
>
>Valice in Sacramento


******************************************************************************
Patrick Hilferty
Belmont, CA 94002
E-Mail:
Web Page: http://home.earthlink.net/~philferty/
*****************************************************************************