I printed this one and kept it (eggplant semi-gloss ^6) 45.7 soda feldspar 15.2 flint 12.7 talc 12.9 gerstley borate 9.0 dolomite 4.5 epk add: 1.0 bentonite 2.0 cobalt carbonate 5.0 manganese carbonate