Joined again after a long absence. I take classes at the Baltimore
Clayworks.

I'm trying to find or re-create a ^10 glaze I once had, called "Sea Foam
Zinc". Does this sound familiar to anyone? Does someone have a recipe
they might share?

Thanks sincerely,
Chris

Tom at Hutchtel.net on sat 8 sep 07


Here's one we've got called Seafoam, probably from CM or John Britt....not
sure...but there's no zinc in it. It's very runny at c10. Can make some
incredible effects though.

Seafoam Green
Code Number: SEAFOAM Cone 10
=========================================

CUSTER FELDSPAR............. 36.00
GERSTLEY BORATE............. 20.00
SILICA...................... 28.00
WHITING..................... 11.00
DOLOMITE.................... 3.00
EPK KAOLIN.................. 2.00
*copper carbonate............ 3.00
=========
103.00


Tom Wirt
Hutchinson, MN
twirt@hutchtel.net
www.claycoyote.com

Eric Suchman on sun 9 sep 07


Looks like it should work at ^6 if I'm interpreting my Glazemaster
correctly.
-Eric in Oceanside


On Sep 8, 2007, at 4:21 PM, Tom at Hutchtel.net wrote:

> Here's one we've got called Seafoam, probably from CM or John
> Britt....not
> sure...but there's no zinc in it. It's very runny at c10. Can
> make some
> incredible effects though.
>
> Seafoam Green
> Code Number: SEAFOAM Cone 10
> =========================================
>
> CUSTER FELDSPAR............. 36.00
> GERSTLEY BORATE............. 20.00
> SILICA...................... 28.00
> WHITING..................... 11.00
> DOLOMITE.................... 3.00
> EPK KAOLIN.................. 2.00
> *copper carbonate............ 3.00
> =========
> 103.00
>
>
> Tom Wirt
> Hutchinson, MN
> twirt@hutchtel.net
> www.claycoyote.com
>
> ______________________________________________________________________
> ________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots2@visi.com