kingl on wed 11 feb 98
Does anyone know of a clay body that is under 3% absorbtion and has a light
to medium orange red color when fired to cone 4?
I have been trying to develop one but I'm running out of time to do so.
Lynette King
Arturo M DeVitalis on thu 12 feb 98
If available in your area, check out Laguna (Millers) # 40.