Donna Maderer on wed 10 mar 99
Does anyone have the recipe for a glaze called "Positive Blue"? It's a cone 10
reduction glaze...I seem to have lost it.
Linda Hughes on sat 9 oct 99
Hi and HELP -
I am in the process of converting from ^10 reduction
firing to ^6 oxidation. In my ^10 work I used an
Oribe, I would love to find a ^6 glaze that will give
the same effect.So far I have been experimenting with
three different bases and have not had any luck yet.
The ^10 Oribe recipe is as follows:
Bone ash 105
Talc 781
Whiting 2236
Custer feldspar 3091
EPK 1255
Flint 2532
Bentonite 200
Black copper oxide
Thanks Always (in advance), Linda R. Hughes
=====