Don Prey on sun 15 aug 99
In a message dated 08/14/99 7:14:52 PM, you wrote:
<thing.. until..i placed cone packs in the kiln to see... and was i
surprised!!! I got a perfect cone 06 bend with a cone 06 in the setter..
>>
That's what I would call a nice calibration result. Certainly well within
the range of possible results for a kiln/setter system. Also of interest is
the present adjustment of the sitter compared to the manufacturers
recommendation. Sitter adjustment and drift over time is one of the biggest
variables. The one thing that we can count on is that things change.
Don Prey in Oregon
| |
|