Wade Blocker on mon 2 oct 00


Andie,
Here is a recipe I really like. It came from Ceramics Monthly,November
91, page 53. The contributors name escapes me, but his initials are M.F.

M.F. Bold Black cone 4 to 6

Dolomite 10.0
Lith carb 2.0
Zinc oxide 1.0
Frit #l4 Hommel 20.5 (I used Ferro 3l34)
Barnard Clay40.0
EPK 13.5
Flint l3.0

add CO carb 3.0
Cu carb 2.0
Rutile 1.0
Titanium dioxide 3.0


Hope this helps, Mia in warm ABQ