karen,
the recipe of this "bisque-glue" :
1/3 corn syrup
1/3 vinegar
1/3 clay ( what you are using)
you can fire it to the temperature of the clay body.
i even use it for porcelain.
good luck,
marta



=====
marta matray gloviczki
rochester,mn
http://users.skynet.be/russel.fouts/Marta.htm