search  current discussion  categories  wanted/for sale - wanted 

looking for black clay body - postscript

updated tue 26 mar 02

 

Wanda Holmes on mon 25 mar 02


Cassius basaltic contains manganese. Use appropriate precautions. wanda

-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
Behalf Of Wanda Holmes
Sent: Sunday, March 24, 2002 6:47 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Looking for Black Clay Body


Aardvark's has a black claybody called Cassius Basaltic. It is a cone 4
body and I have tested it (results available to anyone who wants them). It
gets touchy at cone 5. It is beautiful. They may have a cone 10 black
body, but I'm unaware of it. Wanda

-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
Behalf Of Ilene Mahler
Sent: Sunday, March 24, 2002 12:42 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Looking for Black Clay Body


I believe that Aardvark has such a claybody the I have use in Tom Colemans
workshop...Ilene in Conn
----- Original Message -----
From: Brandon Phillips
To:
Sent: Sunday, March 24, 2002 12:46 AM
Subject: Looking for Black Clay Body


> Hey ya'll, one of my buddies here in abilene is looking for a black clay
> body for cone 10 reduction and/or salt. I've heard in the past that its
not
> possible due to too many oxides, fluxing the body. I may just be crazy.
> Can anyone tell me if this is possible, and maybe have an idea for a
> formula? Any help would be much appreciated!
>
> Brandon Phillips
>
> _________________________________________________________________
> Chat with friends online, try MSN Messenger: http://messenger.msn.com
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at