Janis Young on wed 17 jul 02


Hello, this is my first post to the list although I've
been lurking a month or so. I have an Olympic 2327G
propane kiln I haven't fired for 20+ years and I've
lost all my notes. I'm close to doing a bisque fire
and I wonder if someone who uses this kiln would
suggest a bisque firing schedule, as the manual is
very vague. I have no pyrometer, just cones.

Thanks,
Janis