search  current discussion  categories  wanted/for sale - wanted 

jonathan looking for tig

updated thu 3 jul 03

 

Imbolchottie@AOL.COM on wed 2 jul 03


Some where along the way I lost your email and I have questions re: Celadon
recipe you gave me.

Turned out really nice on the tiles, not so on the plates. I have to go back
and make another batch but I have questions Tig!!
What body do you use it on?
dark or light body?
How did you fire it?
Gas, electric?
Oxidation, reduction?

Thanks again - this is the first glaze I've tried and it's well worth it.
Jonathan in LA

Jennifer Buckner on wed 2 jul 03


At 10:44 AM 7/2/2003, Jonathan in LA wrote:
>Some where along the way I lost your email and I have questions re: Celadon
>recipe you gave me.
>
>Turned out really nice on the tiles, not so on the plates. I have to go back
>and make another batch but I have questions Tig!!
>What body do you use it on?
>dark or light body?
>How did you fire it?
>Gas, electric?
>Oxidation, reduction?


Tig,

If you respond would you do it on-list? I'd love to have a ^6 Celadon recipe.

Thanks,

Jennifer


Jennifer G. Buckner jenniverre@earthlink.net