Crista Nelson on sun 21 may 06


Thank you all for your advice on fixing my crawl spot... The spot was only
the size of a dime but in a very tell, tell spot, but all is well now and
right with the world thanks to all of your advice..... I put a little elmers on
the spot and added some glaze, refired and Wa- La -bam -boom the spot has
disappeared...... Thanks again, Crista