search  current discussion  categories  wanted/for sale - wanted 

for the person looking for a dark green glaze

updated sun 15 oct 06

 

Nancy Braches on sat 14 oct 06


Hi

I was going through my CDs and browsing old copies of clay art back from 98/99 and found a hunter green glaze that I am not sure if anyone has shared with you. It is cone 6 ox and is as follows:

Frit 22%
Strontium Carbonate 16%
Feldspar 34%
Wollastonite 12%
Flint 6%
OM-4 10%

Bentonite 2%
Victoria Green mason stain 8%

it cam from Corcoran School of Art by Grace Lewis

Hope it helps




Nancy